UMARWAN, ARIE (2026) PENGEMBANGAN MATERIAL KOMPOSIT SILIKON ELASTOMER UNTUK ROLLER SILIKON MESIN CAPPING. S2 thesis, Universitas Mercu Buana Jakarta.
|
Text (HAL COVER)
Cover.pdf Download (7MB) | Preview |
|
|
Text (BAB I)
BAB I.pdf Restricted to Registered users only Download (694kB) |
||
|
Text (BAB II)
BAB II.pdf Restricted to Registered users only Download (1MB) |
||
|
Text (BAB III)
BAB III.pdf Restricted to Registered users only Download (885kB) |
||
|
Text (BAB IV)
BAB IV.pdf Restricted to Registered users only Download (1MB) |
||
|
Text (BAB V)
Bab V.pdf Restricted to Registered users only Download (687kB) |
||
|
Text (DAFTAR PUSTAKA)
Dapus.pdf Restricted to Registered users only Download (586kB) |
||
|
Text (LAMPIRAN)
Lampiran.pdf Restricted to Registered users only Download (529kB) |
Abstract
Polydimethylsiloxane (PDMS)-based elastomer using the Room Temperature Vulcanizing (RTV-2) type is widely used in engineering applications due to its flexible and environmentally resistant properties. However, the existing material frequently experiences failures such as fracture, tearing, and cracking, allowing it to withstand only 80,000–130,000 loading cycles. This research aims to develop an RTV-2 PDMS-based elastomer composite with mechanical strength more suitable for withstanding cyclic loading compared to the existing material. The independent variables of the research are the composition of silica fume and clay filler (phr), while the dependent variables are tensile strength and elongation. The research used 27 sampels, with the composition points determined based on a review of prior literature. Data analysis was conducted using the Response Surface Methodology (RSM) to evaluate the effect of filler composition on the mechanical properties of the composite while also determining the optimal composition. The research results show that silica fume increases the composite's mechanical strength up to an optimum composition of 3 phr; addition beyond that limit actually decreases the strength due to particle agglomeration. The best composition obtained experimentally was 3 phr silica fume and 0.1 phr clay, which increased the material's resistance up to 160,805 cycles before failure, while RSM calculations predicted an optimal composition of 6.123 phr silica fume and clay 0.035 phr. The discrepancy between the experimental results and RSM predictions indicates the presence of filler interaction effects that were not fully captured by the model. It can be concluded that the addition of silica fume and clay to the RTV-2 PDMS elastomer composite effectively increases mechanical strength and resistance to cyclic loading, although the filler composition neEDS to be maintained within its optimum limit to avoid performance degradation caused by agglomeration. Keywords: Elastomer composite, RTV-2 , Silica fumed, Clay , RSM Material elastomer berbasis Polydimethylsiloxane (PDMS) tipe Room Temperature Vulcanizing (RTV-2) banyak digunakan pada aplikasi teknik karena sifatnya yang fleksibel dan tahan lingkungan. Namun, material eksisting kerap mengalami kegagalan berupa patah, sobek, dan pecah sehingga hanya mampu bertahan pada rentang 80.000–130.000 siklus beban. Penelitian ini bertujuan mengembangkan komposit elastomer berbasis RTV-2 PDMS dengan kekuatan mekanik yang lebih sesuai untuk menahan beban siklik dibandingkan material eksisting. Variabel bebas penelitian adalah komposisi filler silica fumed dan clay (phr), sedangkan variabel terikatnya adalah tegangan tarik dan elongasi. Penelitian menggunakan 27 sampel, dengan titik komposisi ditentukan berdasarkan kajian literatur terdahulu. Analisis data dilakukan dengan metode Response Surface Methodology (RSM) untuk mengevaluasi pengaruh komposisi filler terhadap sifat mekanik komposit sekaligus menentukan komposisi optimal. Hasil penelitian menunjukkan silica fumed meningkatkan kekuatan mekanik komposit hingga komposisi optimum 3 phr; penambahan melebihi batas tersebut justru menurunkan kekuatan akibat aglomerasi partikel. Komposisi terbaik secara eksperimental diperoleh pada 3 phr silica fumed dan 0,1 phr clay, yang meningkatkan ketahanan material hingga 160.805 siklus sebelum gagal, sementara perhitungan RSM memprediksi komposisi optimal pada 6,123 phr silica fumed dan clay 0,035 phr. Perbedaan hasil eksperimen dan prediksi RSM mengindikasikan adanya efek interaksi antar-filler yang tidak sepenuhnya tertangkap model. Dapat disimpulkan bahwa penambahan silica fumed dan clay pada komposit elastomer RTV-2 PDMS efektif meningkatkan kekuatan mekanik dan ketahanan terhadap beban siklik, namun komposisi filler perlu dijaga pada batas optimum agar tidak terjadi penurunan performa akibat aglomerasi. Kata Kunci : Komposit elastomer, RTV-2, Silica fumed, Clay, RSM